| The
corrosion measuring cells
KMZ 3
and
KMZ 5 are triple electrode
cells for standard electrochemical measurements. Their application fields
mainly are
Corrosion
test
The KMZ 5 is a water-jacketed cell with a cell container suitable for connection to constant temperature circulators. The KMZ 3 is the non-water-jacketed version. The measuring cells have different cell tops with standard taper joints (NS) for the insertion of the working and the counter electrodes, as well as the intermediate vessel with reference electrode and liquid junction tube including a "Haber Luggin capilary". All electrodes have glass bodies with standard tapers. The cells feature a user-friendly handling and a wide range of applications. |
Specifications
|
|
|
|
| Cell container | glass, max. 130 mm in diameter | glass, max. 130 mm in diameter, jacketed with tube connection |
| Capacity | max. 500 ml | max. 500 ml |
| Cell top | about 120 mm in diameter | about 120 mm in diameter |
| Operating temperature | max. 50°C | max. 110°C |
| Specimen holder | PP, NS-29 | PP, NS-29 |
| Counter electrode | NS-24, platinum sheet 4 cm2 | NS-24, platinum sheet 4 cm2 |
| Gas in- and outlet | glass pipe, NS-14.5 | glass pipe, NS-14.5 |
| Reference electrode | KE 10 / NSK 7 (Calomel, 60°C) | KE 10 / NSK 7 (Calomel, 60°C) |
| Liquid junction tube | 2 parts, NS-19 / NS-17, w. Haber Luggin capilary sleeve junctions | 2 parts, NS-19 / NS-17, w. Haber Luggin capilary sleeve junctions |
| Intermediate vessel | glass, NS-29 / 2 x NS-7 | glass, NS-29 / 2 x NS-7 |
| Materials | PVC, PP, glass | PP, glass |
| KMZ
3 and KMZ 5 come with: specimen holder (WE), counter
electrode, reference electrode (Calomel), liquid junction tube, intermediate
vessel, gas in- and outlet.
The following options are available: reference electrode (Ag/AgCl), thermometer, glass stirrer. |
|