AC-DC-AC multichannel

RMUX4

RMUX4 card
The RMUX4 card allows to simultaneously connect up to four electrochemical cells to the potentiostat. The RMUX4 card is designed for corrosion experiments and has high input impedance. The OCP at all channels can be measured simultaneously along with one active channel for e.g., EIS measurement.  Up to four RMUX4 cards can be installed in a ZENNIUM X or ZENNIUM PRO potentiostat which allows simultaneous connection to up to 16 electrochemical cells.
  • Up to 16 channels
  • High input impedance

Specifications

Channels
4 individual
Input voltage range
±4 V / ±10 V
Max. current
±300 mA
Socket
4x Lemosa ERA0S.304 CLL
Input impedance
1 TΩ || 10 pF
Max. RMUX4 supported
4 (16 channels)
Channels
4 individual
Input voltage range
±4 V / ±10 V
Max. current
±300 mA
Socket
4x Lemosa ERA0S.304 CLL
Input impedance
1 TΩ || 10 pF
Max. RMUX4 supported
4 (16 channels)

Downloads

Download the manual about Multicell AC-DC-AC measurements...

Request a quote

Is this the right product for you? Contact our sales team to get further information about our products and their suitability to your individual applications.

Contact Sales
//Cookie Consent by https://www.FreePrivacyPolicy.com //ga code // end of ga code